ViewVC Help
View File | Revision Log | Show Annotations | View Changeset | Root Listing
root/group/trunk/nonperiodicVSS/nonperiodicVSS.tex
(Generate patch)

Comparing trunk/nonperiodicVSS/nonperiodicVSS.tex (file contents):
Revision 3947 by kstocke1, Fri Sep 6 13:09:47 2013 UTC vs.
Revision 3962 by kstocke1, Thu Sep 19 19:42:05 2013 UTC

# Line 285 | Line 285 | Calculated values for the thermal conductivity of a cl
285   \\ \hline \hline
286   {$J_r$} & {$\langle dT / dr \rangle$} & {$\boldsymbol \lambda$}\\
287   {\small(kcal fs$^{-1}$ \AA$^{-2}$)} & {\small(K \AA$^{-1}$)} & {\small(W m$^{-1}$ K$^{-1}$)}\\ \hline
288 + 1.00$\times 10^{-5}$ & 0.38683 & 1.79665486\\
289 + 3.00$\times 10^{-5}$ & 1.1643 & 1.79077557\\
290 + 6.00$\times 10^{-5}$ & 2.2262 & 1.87314707\\
291   \\ \hline \hline
292   \label{table:waterconductivity}
293   \end{longtable}
# Line 294 | Line 297 | Calculated values for the thermal conductivity of a cl
297   %%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
298   \subsection{Interfacial thermal conductance}
299  
300 + The measured interfacial thermal conductance for a 30 \AA$~$ radius gold nanopaticle solvated in TraPPE-UA hexane is 69.55 MW m$^{-2}$ K$^{-1}$. The region A selection was a 25 \AA$~$ radius sphere centered in the nanoparticle and the region B selection was hexane molecules beyond a 67 \AA$~$ radius.
301 +
302   %%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
303   % INTERFACIAL FRICTION
304   %%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%

Diff Legend

Removed lines
+ Added lines
< Changed lines
> Changed lines